À¯¸®¸¦ Á¢ÂøÇÒ ¶§ »ç¿ëÇÏ´Â Á¢ÂøÁ¦ .....With respect to bonding glass we recommend either using the 4463 adhesive Or the 940LE adhesive. If your application reaches and stays at 500F then I would recommend - Testing the 4463 resin with the 4460 hardener as this combination will result In a higher temp version of the 4463. The other option
is to test the 940LE ceramic based adhesive. 260C ÀÌÇÏ¿¡¼ »ç¿ëÇÒ ¶§´Â 4463 ·¹Áø°ú 4460 Çϵå³Ê¸¦ »ç¿ëÇÑ´Ù. »ó¿Â¿¡¼ °æȽÃÅ°´Â °ÍÀÌ ¿°æȺ¸´Ù ³» ÈÇмºÀ» Á¦¿ÜÇÏ°í´Â ¸ðµç ºÎºÐ¿¡¼ ¼º´ÉÀÌ ÁÁ´Ù. 300C ÀÌ»óÀ¸·Î °¡¸é 940LE¸¦ ÀÌ¿ëÇÏ´Â °ÍÀÌ ÁÁ´Ù. 120C¿¡¼ 2½Ã°£ Á¤µµ ±¸¿ö¾ß ÃæºÐÇÑ Àå·ÂÀÌ »ý±ä´Ù. |